Hexcel® HexPly® ES15 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES15 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® ES15 is a modified epoxy matrix specifically designed for rapid curing. It is a structural epoxy for industrial applications requiring a good surface finish and uncomplicated processing.HexPly® ES15 is available with fabric reinforcement.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Cured resin
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 85.0 °C
185 °F
DMA
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 4