Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1900 MPa
276000 psi
Tensile Modulus 124 GPa
18000 ksi
Flexural Yield Strength 2000 MPa
290000 psi
Flexural Modulus 116 GPa
16800 ksi
Compressive Yield Strength 1250 MPa
181000 psi
Shear Strength 80.0 MPa
11600 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 14.0 Month

@Temperature -18.0 °C
14.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 60
Tack Life (days) 30