Hexcel® HexPly® 6268 125°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 6268 125°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® 6268 is a modified epoxy resin which provides good adhesion to honeycomb core. It is a self-extinguishing matrix system offering good toughness, which is used for aircraft primary and secondary structures. HexPly® 6268 is available in UD carbon and woven aramid, glass and carbon.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Cured
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F