Material Notes:
Weight/length = 0.210 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin systems. They are used for weaving, braiding, filament winding applications, unidirectional tapes and prepreg tow for fiber placement. Chopped fibers are used in compression and injection molding compounds to produce machine parts, gears, and chemical valves. The finished products have excellent corrosion, creep and fatigue resistance plus high strength and stiffness characteristics.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4070 MPa
590000 psi
Elongation at Break 1.8 %
1.8 %
Modulus of Elasticity 228 GPa
33100 ksi
Tensile modulus calculated at secant 6000-1000