Henkel Turco Aerowash XTR-1 Jet Cleaner, Exterior Wash

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco Aerowash XTR-1 Jet Cleaner, Exterior Wash.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Turco Aerowash XTR-1 is a silicate-free, VOC-free, water-based, concentrated cleaner, formulated to effectively clean painted and unpainted aircraft exterior surfaces. Turco Aerowash XTR-1 is a gel-type cleaner and is ideally suited for use on all surfaces. Turco Aerowash XTR-1 meets the standards of AMS 1523A Cleaner for Exterior Aircraft Surface Thickened or Gel-Type, Water-based.Application: Aircraft Appearance
Descriptive Properties Value Comments
Chemistry Alkaline, Water-based
Consistency Liquid
Form Concentrated