Henkel Turco Aerowash Jet Cleaner, Exterior Wash

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco Aerowash Jet Cleaner, Exterior Wash.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Turco Aerowash is a concentrated liquid all-purpose maintenance cleaner. It contains a unique blend of alkaline materials, solvents and surfactants, which makes this product highly effective against a wide variety of soils. Turco Aerowash is safe to use on all metals, glass, painted surfaces and plastics.Application: Aircraft Appearance
Descriptive Properties Value Comments
Chemistry Alkaline, Water-based
Consistency Liquid
Form Concentrated
Substrate Aluminum
Ferrous
Magnesium
Non-Ferrous
Stainless Steel
Titanium