Material Notes:
Turco 4215 NC-LT is a white granular mix developed for cleaning ferrous and nonferrous alloys by spray, immersion and ultrasonic methods at low temperatures. Ideal for cleaning fuel and hydraulic components and for cleaning metals prior to metal bonding.Applications:Alkaline EtchConversion CoatingsBoric Sulfuric Anodizing Chromic Acid Anodizing Phosphoric Acid Anodizing
Processing Properties Metric English Comments
Processing Temperature 49.0 - 60.0 °C

@Time 900 sec
120 - 140 °F

@Time 0.250 hour
Immersion
Descriptive Properties Value Comments
Chemistry Alkaline
Water-based
Consistency Powder
Form Concentrated
Substrate Aluminum
Ferrous
Stainless Steel
Titanium