Material Notes:
Expanding modified epoxy film, cures at 250°F / 121°C, used for jet engine abradable fan seals.
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 7.60 MPa
1100 psi
Tensile Modulus 0.430 GPa
62.4 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 121 °C
2.00 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Out-Time (days) 10
at 32°C
15
at 25°C