Material Notes:
Ridoline 298 is a liquid, non-silicated, immersion cleaner for aluminum and aluminum alloys. It is formulated for use in anodizing and conversion coating lines. It is free rinsing and will remove a variety of soils including oils, greases, inks, and wax-based markings.Applications: Alkaline Etch Conversion CoatingsBoric Sulfuric Anodizing Chromic Acid Anodizing Phosphoric Acid Anodizing
Processing Properties Metric English Comments
Processing Temperature 54.0 - 82.0 °C

@Time 900 sec
129 - 180 °F

@Time 0.250 hour
Immersion
Descriptive Properties Value Comments
Chemistry Alkaline
Water-based
Consistency Liquid
Form Concentrated
Substrate Aluminum
Titanium