Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified BMI foaming core splice, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs. Elevated service temperature to 450°F / 232°C.
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.90 MPa

@Temperature 25.0 °C
1000 psi

@Temperature 77.0 °F
tube shears
6.90 MPa

@Temperature 121 °C
1000 psi

@Temperature 250 °F
tube shears
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 232 °C
2.00 hour

@Temperature 450 °F
Descriptive Properties Value Comments
Out-Time (days) 10
at 32°C
30
at 25°C