Henkel Hysol EA 9657 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9657 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temperature, service film adhesive designed for high honeycomb peel in a reticulated sound suppression structure. Qualified to BMS 5-137. Data from .080 psf, 400 g / m2.Applications: Composite Bonding Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 8.00 MPa
1160 psi
Flatwise
Adhesive Bond Strength 15.9 MPa

@Temperature 177 °C
2310 psi

@Temperature 351 °F
Lap Shear
33.0 MPa

@Temperature -55.0 °C
4790 psi

@Temperature -67.0 °F
Lap Shear
34.5 MPa

@Temperature 25.0 °C
5000 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Glass Transition Temp, Tg 132 °C
270 °F
wet
182 °C
360 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 60
at 25°C
Out-Time (days) 15
at 25°C