A water-based cleaner for composite and metal molds. The surfactants and emulsifiers in combination with soft abrasives give excellent cleaning results without dulling or scratching the surface.Benefits: Water-based polishing liquid, Removes cured films
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.0 °C
104 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 25.0 °C
0.0833 hour

@Temperature 77.0 °F