Henkel Alodine 871 Touch-N-Prep Coating Touch-Up Conversion Coating

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Alodine 871 Touch-N-Prep Coating Touch-Up Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alodine 871 Touch-N-Prep Coating is a non-hexavalent chromium dry-in-place conversion coating designed for use on aluminum and its alloys. The applicator used to deliver this product provides an easy and safe method of repairing bare areas of aluminum surfaces. Alodine 871 is formulated for both bare corrosion protection such as ASTM 921-02 and bonding applications when combined with organic coatings or structural adhesives.
Processing Properties Metric English Comments
Processing Temperature 23.0 °C
73.4 °F
Descriptive Properties Value Comments
Chemistry Tri-Chrome
Consistency Liquid
Form Ready-to-Use
Substrate Aluminum