Henkel Alodine 1600 / Alodine 1660 Additive Conversion Coating

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Alodine 1600 / Alodine 1660 Additive Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alodine 1600 is a concentrated, liquid two-package chemical used to produce a chromate conversion coating on aluminum and all its alloys. The color ranges from light iridescent gold to tan. Alodine 1600 does not contain complex cyanides.
Descriptive Properties Value Comments
Chemistry Chromate
Consistency Liquid
Form Concentrated, Two Part
Substrate Aluminum