Material Notes:
The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 142 °C
288 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range