Heatbath/Park High Temp Draw Salt Quenching and Tempering Salt

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park High Temp Draw Salt Quenching and Tempering Salt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Salt mixture particularly suitable for ausquenching/austempering. (430 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 249 °C
480 °F
Lower limit of working range