Heatbath/Park Durastrip M-3 Cleaning Salt

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park Durastrip M-3 Cleaning Salt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A highly alkaline and oxidizing salt bath mixture that will rapidly strip all types of paint. Enamels, lacquers, varnishes, porcelain enamels and all other types of paint, including hard to strip epoxy coatings, are rapidly and completely removed from ferrous metals.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 288 °C
550 °F
Maximum Service Temperature, Air 482 °C
900 °F
Upper limit of working range
Minimum Service Temperature, Air 399 °C
750 °F
Lower limit of working range