Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UL, Inc. has granted HST-II the highest thermal recognition ever achieved by any glass polyester laminate (U.L. File No. E81893). HST-II has a 220º C/210º C rating for 1/8" thick and heavier, and a 210º C/210º C rating for 1/32" thick up to 1/8" thick. HST-II is a high temperature polyester laminate that exhibits excellent retention of electrical and mechanical properties at elevated temperatures. Applications for HST-II can be found in high voltage transformers, D.C. motors and elsewhere when materials with high thermal indices are required. Available thicknesses - .031" - 2.00". Standard color - Brown.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D572
Water Absorption 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 52
52
Tensile Strength, Ultimate 90.0 MPa
13100 psi
Flexural Strength 172 MPa
24900 psi
Flexural Modulus 12.0 GPa
1740 ksi
Compressive Strength 228 MPa
33100 psi
Shear Strength 97.0 MPa
14100 psi
ASTM D732
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Approximate temperature class
Flammability, UL94 HB
HB
File No.E81893
Electrical Properties Metric English Comments
Dielectric Constant 4.2

@Frequency 60 Hz
4.2

@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm

@Thickness 1.59 mm
483 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil and Air; ASTM D149
Dissipation Factor 0.010

@Frequency 60 Hz
0.010

@Frequency 60 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index >= 500 V
>= 500 V