Haysite H515 Polyester, High Temp Flex

Category Polymer , Thermoset , Polyester, TS
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite H515 Polyester, High Temp Flex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high temperature is required. Standard color is tan. Thickness is 1/32" - 1/16". Sheet sizes are 36" x 72" and 48" x 96".Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Water Absorption 1.1 %
1.1 %
ASTM D229
Mechanical Properties Metric English Comments
Tensile Strength 42.7 MPa
6200 psi
LW; ASTM D638
46.2 MPa
6700 psi
CW; ASTM D638
Compressive Strength 74.5 MPa
10800 psi
Flatwise; ASTM D695
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Edgewise (CW); ASTM D256
5.34 J/cm
10.0 ft-lb/in
Edgewise (LW); ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Elec.
200 °C
392 °F
Mech.
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 5.2

@Frequency 60.0 Hz
5.2

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
560 kV/in
Perpendicular, short time in air; ASTM D149
23.6 kV/mm
600 kV/in
Perpendicular, short time in oil; ASTM D149
Dissipation Factor 0.057

@Frequency 60.0 Hz
0.057

@Frequency 60.0 Hz
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495