Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plates and terminal boards. Available in thicknesses - .032" - 2.00". Standard color - Brown. Meets Gov't Specs - LP-509, I-24768/6.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D572
Water Absorption 0.31 %
0.31 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 74
74
Tensile Strength, Ultimate 90.0 MPa
13100 psi
Flexural Strength 186 MPa
27000 psi
Flexural Modulus 11.8 GPa
1710 ksi
Compressive Strength 379 MPa
55000 psi
Shear Strength 124 MPa
18000 psi
ASTM D732
Izod Impact, Notched 6.10 J/cm
11.4 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Approximate temperature class
Electrical Properties Metric English Comments
Dielectric Constant 4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
ASTM D150
4.67

@Frequency 60 Hz
4.67

@Frequency 60 Hz
ASTM D150
Dielectric Strength 13.0 kV/mm

@Thickness 1.59 mm
330 kV/in

@Thickness 0.0625 in
Perpendicular, Short Time in Oil and Air; ASTM D149
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
ASTM D150
0.019

@Frequency 60 Hz
0.019

@Frequency 60 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Copyright © lookpolymers.com All Rights Reserved