Haysite 54500 Polyester SMC, 35% Glass Reinforced

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 54500 Polyester SMC, 35% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, and has a UL94 Flame Class V-0.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D572
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 128 MPa
18600 psi
Flexural Strength 248 MPa
36000 psi
Compressive Strength 145 MPa
21000 psi
Izod Impact, Notched 12.8 J/cm
24.0 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 185 sec
185 sec
ASTM D495