Material Notes:
The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electrical properties after exposure to elevated temperatures.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D572
Water Absorption 0.235 %
0.235 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
Flexural Strength 172 MPa
24900 psi
Compressive Strength 103 MPa
14900 psi
Izod Impact, Notched 10.7 J/cm
20.0 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Strength 17.0 kV/mm
432 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 100 sec
100 sec
ASTM D495