Material Notes:
The 43000 series sheet molding compound is a general purpose material. Designed for compression molding, this grade exhibits good mechanical properties and resistance to mild corrosive agents.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D572
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
Flexural Strength 172 MPa
24900 psi
Compressive Strength 103 MPa
14900 psi
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Constant 4.6

@Frequency 60 Hz
4.6

@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.0030

@Frequency 60 Hz
0.0030

@Frequency 60 Hz
ASTM D150
Arc Resistance 140 sec
140 sec
ASTM D495