Material Notes:
Haysite Grade 42100 is a fiber glass reinforced thermoset polyester sheet molding compound exhibiting excellent moldability. It is designed for compression molded parts requiring high strength and good electrical properties.
Physical Properties Metric English Comments
Density 1.84 g/cc
0.0665 lb/in³
ASTM D572
Water Absorption 0.16 %
0.16 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
14900 psi
Flexural Strength 152 MPa
22000 psi
Compressive Strength 124 MPa
18000 psi
Izod Impact, Notched 9.80 J/cm
18.4 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Flammability, UL94 V-0
V-0
File No.E-27875
Electrical Properties Metric English Comments
Dielectric Constant 5.2

@Frequency 60 Hz
5.2

@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
Perpendicular (ASTM D149), Short Time
Dissipation Factor 0.0189

@Frequency 60 Hz
0.0189

@Frequency 60 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Users viewing this material also viewed the following: