Material Notes:
Haysite 30000 series bulk molding compound is a general purpose material. This compound can be compression, transfer, or injection molded. This material has good mechanical properties and can be pigmented to a wide range of industrial colors.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D572
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
Flexural Strength 103 MPa
14900 psi
Compressive Strength 103 MPa
14900 psi
Izod Impact, Notched 3.70 J/cm
6.93 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 180 sec
180 sec
ASTM D495