Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC , Vinyl Ester
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compression, transfer, or injection molded.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
ASTM D572
Water Absorption 0.29 %
0.29 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
Flexural Strength 159 MPa
23100 psi
Compressive Strength 145 MPa
21000 psi
Izod Impact, Notched 5.90 J/cm
11.1 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Electrical Properties Metric English Comments
Dielectric Strength 15.0 kV/mm
381 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 187 sec
187 sec
ASTM D495