Haveg 61NA Furfuryl Alcohol-Formaldehyde Resin

Category Polymer , Thermoset
Manufacturer Haveg
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haveg 61NA Furfuryl Alcohol-Formaldehyde Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A proprietary thermoset plastic consisting of a furfuryl alcohol-formaldehyde resin and non-asbestos silicate fillers.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Moisture Absorption at Equilibrium 2.65 %
2.65 %
No Time Specified
Moisture Vapor Transmission 0.990 cc-mm/m²-24hr-atm
2.51 cc-mil/100 in²-24hr-atm
g/cm²-atm (no time specified)
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.8 MPa
5050 psi
Elongation at Break 0.84 %
0.84 %
Tensile Modulus 6.80 GPa
986 ksi
Flexural Yield Strength 63.8 MPa
9250 psi
Compressive Yield Strength 140 MPa
20300 psi
Izod Impact, Notched 0.360 J/cm
0.674 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 24.3 µm/m-°C

@Temperature 20.0 °C
13.5 µin/in-°F

@Temperature 68.0 °F