Hannam Chemical Hanalac 740 ABS, Super High Impact Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac 740 ABS, Super High Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Superior impact strength, even at low temperature. Applications: helmets, shoe heels, bobbins, roller skates, bags, pipes, radiator grills, auto parts, appliance wheels.
Physical Properties Metric English Comments
Melt Flow 2.1 g/10 min
2.1 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Yield Strength 59.0 MPa
8560 psi
ASTM D790
Flexural Modulus 2.05 GPa
297 ksi
ASTM D790
Izod Impact, Notched 3.60 J/cm

@Thickness 3.17 mm
6.74 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Flammability, UL94 HB
HB