Material Notes:
Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC)
Physical Properties Metric English Comments
Particle Size 1.0 - 1.5 µm
1.0 - 1.5 µm
Average
1.0 - 3.0 µm
1.0 - 3.0 µm
Laser Diffraction D50
Component Elements Properties Metric English Comments
Carbon, C >= 19.2 %
>= 19.2 %
Free C <= 0.50 %
<= 0.50 %