Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Molybdenum Alloy AB-30W Arc-Cast Bar

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Molybdenum Alloy AB-30W Arc-Cast Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description of Product: This specification covers wrought bar of carbon-deoxidized molybdenum 30% tungsten alloy produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting process.Structure: The bar will be supplied in the stress-relieved condition. Material can also be supplied in the recrystallized condition.Information provided by H.C. Starck.
Mechanical Properties Metric English Comments
Hardness, Vickers 230 - 290

@Load 10.0 kg,
Diameter 28.57 - 34.92 mm
230 - 290

@Load 22.0 lb,
Diameter 1.125 - 1.375 in
mid-radius; DPH (10 kg)
230 - 290

@Load 10.0 kg,
Diameter 34.92 - 73.03 mm
230 - 290

@Load 22.0 lb,
Diameter 1.375 - 2.875 in
mid-radius; DPH (10 kg)
235 - 300

@Load 10.0 kg,
Diameter 22.2 - 28.57 mm
235 - 300

@Load 22.0 lb,
Diameter 0.875 - 1.125 in
mid-radius; DPH (10 kg)
240 - 300

@Load 10.0 kg,
Diameter 3.17 - 22.2 mm
240 - 300

@Load 22.0 lb,
Diameter 0.125 - 0.875 in
mid-radius; DPH (10 kg)
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Iron, Fe <= 0.0080 %
<= 0.0080 %
Molybdenum, Mo >= 66.9 %
>= 66.9 %
by difference
Nickel, Ni <= 0.0020 %
<= 0.0020 %
Nitrogen, N <= 0.0020 %
<= 0.0020 %
Oxygen, O <= 0.0025 %
<= 0.0025 %
Silicon, Si <= 0.0080 %
<= 0.0080 %
Tungsten, W 27 - 33 %
27 - 33 %
Copyright © lookpolymers.com All Rights Reserved