H.C. Starck MoMP 4.5 - 5.5 micron Molybdenum Metal Powder, Mo (99.95%)

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal , Pure Element
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck MoMP 4.5 - 5.5 micron Molybdenum Metal Powder, Mo (99.95%).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description of Product: Grey metal powder. Sieved.Typical Applications: The production of pressed and sintered Mo or Mo alloy parts. Also used to produce blended alloy powders.Information provided by H.C. Starck.
Physical Properties Metric English Comments
Particle Mesh Size 230 Mesh
230 Mesh
screening fraction max 0.5%; Sieve Analysis per ASTM B214
Component Elements Properties Metric English Comments
Chromium, Cr <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.0050 %
<= 0.0050 %
Magnesium, Mg <= 0.0010 %
<= 0.0010 %
Molybdenum, Mo >= 99.95 %
>= 99.95 %
excluding gases
Nickel, Ni <= 0.0020 %
<= 0.0020 %
Oxygen, O <= 0.10 %
<= 0.10 %
Potassium, K <= 0.0060 %
<= 0.0060 %
Silicon, Si <= 0.0030 %
<= 0.0030 %
Tin, Sn <= 0.0030 %
<= 0.0030 %
Descriptive Properties Value Comments
Fisher Number 4.5 to 5.5 µm