Material Notes:
Alpha phase > 84%. Standard and cost effective grade.Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high precision ballsSiAlONsMetallurgy (thermocouple protection tubes, stalk tubes, crucibles)Chemical engineering, e.g. heat exchangersFunctional parts in textile machineryReleasing agent in Silicon ingot production
Physical Properties Metric English Comments
Particle Size 1.5 µm
1.5 µm
Average Particle Size/Laser Diffraction D50