H.C. Starck Grade A Zirconium Carbide, ZrC

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade A Zirconium Carbide, ZrC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Additive for hard metalsAdditive for powder metallurgyModerator in solid fuel propellant
Physical Properties Metric English Comments
Particle Size 5.0 - 9.0 µm
5.0 - 9.0 µm
Laser Diffraction D50
<= 20 µm
<= 20 µm
90% less than
Component Elements Properties Metric English Comments
Hafnium, Hf <= 2.0 %
<= 2.0 %