H.C. Starck Cobalt and Cobalt Hardfacing Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy , Pure Element
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Cobalt and Cobalt Hardfacing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cobalt water atomized as alloying intermediates for sintering magnets and other P/M-parts. Co-HFA (Hard Facing Alloys) against metal-to-metal wear, corrosion, erosion and hot abrasion for extruder screws, pump shafts, wear rings, valve seats and discs.
Component Elements Properties Metric English Comments
Carbon, C <= 0.30 %
<= 0.30 %
Cobalt, Co >= 99 %
>= 99 %
Iron, Fe <= 0.20 %
<= 0.20 %
Nickel, Ni <= 0.30 %
<= 0.30 %
Other <= 0.040 %
<= 0.040 %