Material Notes:
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
Viscosity 26 cP

@Temperature 21.0 °C
26 cP

@Temperature 69.8 °F
Thermal Properties Metric English Comments
Melting Point 21.0 °C
69.8 °F
Decomposition Temperature 267 °C
513 °F
100 mbar
Descriptive Properties Value Comments
Color none