H.C. Starck Amperit® 585.3 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 585.3 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Composition is of Cr3C2 only
Physical Properties Metric English Comments
Particle Size 5.5 µm
5.5 µm
Maximum of 10% less than, Cr3C2
5.5 µm
5.5 µm
Maximum of 10% less than, NiCr
45 µm
45 µm
Maximum of 7% greater than, NiCr
62 µm
62 µm
minimum of 95% less than, Cr3C2
88 µm
88 µm
100% less than, Cr3C2
Component Elements Properties Metric English Comments
Carbon, C >= 12.75 %
>= 12.75 %
Chromium, Cr <= 87.25 %
<= 87.25 %
Iron, Fe <= 0.70 %
<= 0.70 %
Silicon, Si <= 0.10 %
<= 0.10 %