Material Notes:
HS Number: 28499030
Physical Properties Metric English Comments
Particle Size 45 µm
45 µm
Maximum of 10% less than
90 µm
90 µm
Maximum of 5% greater than
Component Elements Properties Metric English Comments
Carbon, C 4.8 - 5.2 %
4.8 - 5.2 %
Cobalt, Co 16 - 18 %
16 - 18 %
Iron, Fe <= 2.0 %
<= 2.0 %