H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 5.00 - 5.60 g/cc
0.181 - 0.202 lb/in³
ASTM B212
Particle Size 17 - 21 µm
17 - 21 µm
10%
30 - 38 µm
30 - 38 µm
50%
53 - 63 µm
53 - 63 µm
90%
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 5.2 - 5.6 %
5.2 - 5.6 %
Cobalt, Co 11 - 13 %
11 - 13 %
Iron, Fe <= 0.20 %
<= 0.20 %
Tungsten, W 81.2 - 83.8 %
81.2 - 83.8 %