H.C. Starck Amperit® 512.059 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 512.059 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 3.80 - 4.60 g/cc
0.137 - 0.166 lb/in³
ASTM B417
Particle Size 7.0 - 12 µm
7.0 - 12 µm
10%
14 - 19 µm
14 - 19 µm
50%
25 - 35 µm
25 - 35 µm
90%
Component Elements Properties Metric English Comments
Carbon, C 3.9 - 4.3 %
3.9 - 4.3 %
Cobalt, Co 10 - 12 %
10 - 12 %
Iron, Fe <= 0.30 %
<= 0.30 %