H.C. Starck Amperit® 410.1 Gas Atomized (NiCoCrAlY)

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 410.1 Gas Atomized (NiCoCrAlY).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 22 µm
22 µm
Maximum of 15% less than
45 µm
45 µm
Maximum of 7% greater than
Component Elements Properties Metric English Comments
Aluminum, Al 11.5 - 13.5 %
11.5 - 13.5 %
Chromium, Cr 15 - 19 %
15 - 19 %
Cobalt, Co 20 - 26 %
20 - 26 %
Nickel, Ni 40.8 - 53.3 %
40.8 - 53.3 %
Yttrium, Y 0.20 - 0.70 %
0.20 - 0.70 %