H.C. Starck Amperit® 235.091 Calcined Bentonite coated with Nickel-Chromium-Aluminum

Category Ceramic
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 235.091 Calcined Bentonite coated with Nickel-Chromium-Aluminum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 45 µm
45 µm
Maximum of 5% less than
150 µm
150 µm
Maximum of 2% greater than
Component Elements Properties Metric English Comments
Aluminum, Al 1.0 - 6.0 %
1.0 - 6.0 %
Chromium, Cr 1.5 - 6.5 %
1.5 - 6.5 %
Nickel, Ni 63.5 - 79.5 %
63.5 - 79.5 %
Descriptive Properties Value Comments
Bentonite (leached), wt % 18-24