Material Notes:
Composition is of NiSF RC 60 only
Physical Properties Metric English Comments
Apparent Bulk Density 2.20 - 2.90 g/cc
0.0795 - 0.105 lb/in³
Mo; ASTM B212
3.80 - 4.60 g/cc
0.137 - 0.166 lb/in³
NiSF RC 60; ASTM B212
Particle Size 20 µm
20 µm
Maximum of 3% less than, (NiSF RC 60)
45 µm
45 µm
Maximum of 30% less than, (Mo)
45 µm
45 µm
Maximum of 30%, Mo
53 µm
53 µm
Maximum of 10% greater than, (NiSF RC 60)
90 µm
90 µm
Maximum of 5% greater than, (Mo)
Component Elements Properties Metric English Comments
Boron, B 3.0 - 3.9 %
3.0 - 3.9 %
Carbon, C 0.60 - 1.2 %
0.60 - 1.2 %
Chromium, Cr 13 - 17 %
13 - 17 %
Iron, Fe 2.4 - 4.6 %
2.4 - 4.6 %
Nickel, Ni 68.4 - 77.1 %
68.4 - 77.1 %
Silicon, Si 3.9 - 4.9 %
3.9 - 4.9 %