Gwent Electronic Materials D2070209P6 White Dielectric Paste

Category Fluid , Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials D2070209P6 White Dielectric Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties. Excellent adhesion to ITO, chemical and environmental resistance. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-325tpiSubstrate: ITO coated polyesterInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 73.5 - 76.5 %

@Temperature 150 °C
73.5 - 76.5 %

@Temperature 302 °F
Viscosity 1400 - 2300 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
1400 - 2300 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 20.0 microns
0.787 mil
Double layer on 175µm ITO coated polyester
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
10.0 min

@Temperature 130 °C
0.167 hour

@Temperature 266 °F
box oven
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 242
1st layer, Using a 230 mesh stainless steel screen
260
2nd layer, Using a 230 mesh stainless steel screen
Users viewing this material also viewed the following: