Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2091208D1 Carbon Graphite Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2091208D1 Carbon Graphite Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is designed to be used for screen printing working electrodes. It gives excellent electrochemical performance with good reversibility when using cyclic voltammetry. The ink should be gently stirred before use avoiding introduction of air bubbles. This ink can be used in conjunction with UV dielectrics, good for large volume printing, and ink is very slow drying for faster drying please see C2030519P4. Screen Printing Equipment: automatic, semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230 tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 41 - 43 %

@Temperature 130 °C
41 - 43 %

@Temperature 266 °F
Viscosity 5000 - 8000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
5000 - 8000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 16.7 microns
0.657 mil
Cured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 59 ohm

@Thickness 0.0167 mm
59 ohm

@Thickness 0.000657 in
Typical, Printed through 230 stainless steel mesh with 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 236
Using a 230 mesh stainless steel screen
Copyright © lookpolymers.com All Rights Reserved