Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2021031D3 Electrode Ink

Category Fluid , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2021031D3 Electrode Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is designed for printing on PVB tape.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 70 %
70 %
Particle Size <= 2.0 µm
<= 2.0 µm
Main Break; Fineness of Grind
<= 4.0 µm
<= 4.0 µm
3rd Streak; Fineness of Grind
Viscosity 17300 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
17300 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C
68.0 °F
Processing Properties Metric English Comments
Cure Time <= 1.98 min

@Temperature 150 °C
<= 0.0330 hour

@Temperature 302 °F
touch dry
<= 4.02 min

@Temperature 75.0 °C
<= 0.0670 hour

@Temperature 167 °F
touch dry
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 160
230 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens
Users viewing this material also viewed the following: