Guarniflon PFA Perfluoroalkoxy Polymer

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Guarniflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon PFA Perfluoroalkoxy Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for applications up to 260°C. Thanks to its fluidity during the processing, the final products in PFA - especially the skived film - are absolutely porous-free, hence very suitable for electrical applications.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ASTM D2240
Tensile Strength >= 30.0 MPa
>= 4350 psi
ASTM D638
Elongation at Break >= 380 %
>= 380 %
ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
25°C to 100°C; ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM D177
Melting Point 300 - 310 °C
572 - 590 °F
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
ASTM D149