Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Guarniflon MFA Fluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer , TFE/Perfluoromethylvinylether Copolymer (MFA)
Manufacturer Guarniflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon MFA Fluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It is an ideal choice for extreme thermal and chemical environments. MFA exhibits the outstanding thermal behaviour and chemical resistance found in PTFE, PFA and FEP. In addition, parts made with MFA have been shown to have smooth finished surfaces. This makes MFA a good candidate for the semiconductor, electronics and biologic applications.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.12 - 2.17 g/cc
0.0766 - 0.0784 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ASTM D2240
Tensile Strength >= 25.0 MPa
>= 3630 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
25°C to 100°C; ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM D177
Melting Point 260 - 290 °C
500 - 554 °F
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
ASTM D149