Grupo Repol Dinalon® B1S25 N Fast Cycling, Nucleated Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Nucleated
Manufacturer Grupo Repol
Trade Name Dinalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Grupo Repol Dinalon® B1S25 N Fast Cycling, Nucleated Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Flexural Strength 105 MPa
15200 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched <= 1.00 J/cm²

@Temperature 23.0 °C
<= 4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50 N; ISO 306