Material Notes:
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ISO 527
Elongation at Break 6.0 %
6.0 %
ISO 527
Elongation at Yield 2.5 %
2.5 %
ISO 527
Tensile Modulus 7.20 GPa
1040 ksi
ISO 527
Flexural Strength 135 MPa
19600 psi
ISO 178
Flexural Modulus 4.80 GPa
696 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50N; ISO 306