Material Notes:
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527
Elongation at Break 20 %
20 %
ISO 527
Elongation at Yield 3.5 %
3.5 %
ISO 527
Tensile Modulus 2.80 GPa
406 ksi
ISO 527
Flexural Strength 90.0 MPa
13100 psi
ISO 178
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched <= 1.00 J/cm²

@Temperature 23.0 °C
<= 4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50N; ISO 306